Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL PPX™ Resin PPX640F - Americas - (PPE+PP)-GF40 - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL PPX™ Resin PPX640F - Americas:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Noryl PPX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
NORYL PPX™ 640F resin is a 40% glass reinforced alloy of polyphenylene ether (PPE) + polypropylene (PP). This injection moldable grade is NSF 61 certified and exhibits high elongation and stiffness along with temperature performance, impact resistance, hydrolytic and dimensional stability. NORYL PPX640F resin is an excellent candidate for copper and brass replacement in water management applications such as water filtration systems, boiler systems, and heat exchangers.

UL Yellow Card Link E121562-221228
Processing/Physical Characteristics단위시험규격
ASTM 데이터
용융 흐름성, MFI 1.3 g/10min ASTM D 1238
온도 260 °C -
하중 5 kg -
기계적 특성단위시험규격
ASTM 데이터
항복강도 95 MPa ASTM D 638
파단시 강도 95 MPa ASTM D 638
파단시 신율 6.4 % ASTM D 638
굴곡 계수 8310 MPa ASTM D 790
아이조드 충격은 노치, 1/8 in 106 J/m ASTM D 256
아이조드 충격은 노치, Low-Temperature 96 J/m ASTM D 256
온도 -30 °C -
Izod충격강도, 1/8 in 576 J/m ASTM D 256
열적 특성단위시험규격
ISO 데이터
1.5mm 평균두께에서의 난연성 HB class IEC 60695-11-10
테스트 두께 1.5 mm -
ASTM 데이터
DTUL @ 66 psi 158 °C ASTM D 648
DTUL @ 264 psi 146 °C ASTM D 648
비카트 연화 온도 163 °C ASTM D 1525
기타 특성단위시험규격
밀도 1300 kg/m³ ASTM D 792
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 65 - 75 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.02 % -
용융수지온도 260 - 305 °C -
성형온도 40 - 65 °C -
Zone 1 245 - 290 °C -
Zone 2 250 - 290 °C -
Zone 3 255 - 300 °C -
Screw speed 20 - 100 rpm -
Back pressure 0.3 - 0.7 MPa -
특징
생산 공정
사출 성형
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.